Bill Roberts (not verified) -
Saturday, May 12, 2007 - 9:49am
I also like the phos copper rod, or the TIG option. IF you have a TIG.......you can just cut lil strips of the copper to use as filler.
As for these processes annealing your copper. One way to reharden your copper is to "Bead blast" it in a cabinet. IF you use glass beads it leaves a very nice finish and work hardens the copper.
Bill
Reply
Welding
You must login/register in order to contribute to this group.
Random image
who is chatting
Who's online
There are currently 0 users and 106 guests online.
I also like the phos copper
I also like the phos copper rod, or the TIG option. IF you have a TIG.......you can just cut lil strips of the copper to use as filler.
As for these processes annealing your copper. One way to reharden your copper is to "Bead blast" it in a cabinet. IF you use glass beads it leaves a very nice finish and work hardens the copper.
Bill